| CuNi3Si | Mechanical Properties | |
|---|---|---|
| 1 | Hardness | 220 -240 HB |
| 2 | Yield Strength | 650 - 750 N/mm2 |
| 3 | Tensile Strength | 750 - 850 N/mm2 |
| 4 | Elongation | 6 - 10 % |
| CuNi3Si | Physical Properties | |
|---|---|---|
| 1 | Electrical Conductivity | 25 %MS/m |
| 2 | Thermal Conductivity | 17 W/mK |
| 3 | Density | 8.8 g/cm3 |